The series of experiments was made to get knowledge about
the hardness acceptance and crystalline structures at the material X165CrV12.
Initial condition : hot rolled 14,00 mm , unpickled Heat treatment
: laboratory furnace (volume 2 liter)
Hardening : holding time 30 minutes , quenching in oil and air
Tempering : holding time 90 minutes , cooling at air